• Security six laminates

    • Material:FR4
      Layer:6
      Board thickness:1.6mm
      Copper weight: 1oz
      Min trace width/spacing: 0.076/0.076mm
      Min hole size:0.2mm
      Surface finish:Immersion Gold + Hard Gold
      Specialty:Hard Gold Finger 30U
      Application:Security